CHEMICAL ANALYSIS

SiO21.22%
Al2O30,72%
Fe2O3 total0.28%
MnOvest.
CaO51.65%
MgO 2.76%
Na2O0.07%
K2O 0.22%
TiO243.25
CO243.54

PHYSICAL-MECHANICAL CHARACTERISTICS

Compressive strength ( Kg/cm²) 930
Compressive strength after ice ( kg/cm² )962
Resistance to bending ( kg/cm²) 193
Apparent volumetric mass (kg/cm²)2726
Water absorption PTN 0.08%
Open porosity 0.21%
Coefficient of linear expansion ( 106/ºC)7.2
Amsler Wear (mm)1.4
Shock resistance ( cm)50

FINISHING

  • Polished
  • Honed
  • Sandblasted
  • Bush-hammered
  • Split
  • Brushed

RECOMENDED APPLICATIONS

Exterior

Interior